Post by revver on Feb 2, 2015 23:01:39 GMT
it does say on the tin that simoniz needs to be baked in the over to be solvent resistant, but even then petrol fetches it off in seconds. Hammerite isn't much better either. dont say that, i've got 5 cans in the shed waiting to be used.
|
|
|
Post by scott on Feb 2, 2015 23:02:48 GMT
I'm always careful but sometimes accidents happen.
I am going to have to extra careful with my SB200 though, the tank is painted with hammerite smooth blue! It was cellulose (still is underneath) and that does start to melt with petrol if not wiped off but hammerite paint will be off in an instant.
|
|
Deleted
Deleted Member
Posts: 0
|
Post by Deleted on Feb 2, 2015 23:02:53 GMT
You could always paint the shed with it, Kev..
|
|
|
Post by scott on Feb 2, 2015 23:04:15 GMT
there is little but powder coat and 2K that doesn't come off with petrol - even halfords petrol resistant lacquer isn't petrol resistant
|
|
|
Post by revver on Feb 2, 2015 23:29:48 GMT
You could always paint the shed with it, Kev.. or i could paint the wheels with it nick.
|
|
Deleted
Deleted Member
Posts: 0
|
Post by Deleted on Feb 3, 2015 13:17:48 GMT
Could do.... I think we should all remember something though - the original paint was pretty crap as well.....So if you want originality, it should not be that durable and also not resistant to anything.....makes sense? Don't over restore 'em.
|
|